          Material Groups                                            Recommended Machining Conditions

                                                                                       Feed vs. Drill Diameter


                                                   Tensile                        D=12-13.9  D=14-15.9  D=16-17.9  D=18-19.9  D=20-21.9  D=22-23.9  D=24-25.9  INDEXABLE DRILLS
                                                  Strength
                                                    Rm    Hardness  Mtl.   VC
           ISO   Material              Condition   [N/mm ]  HB    No.   m/min               mm/rev
                                                       2
                           < 0.25 %C    Annealed    420     125    1
                           ≥ 0.25 %C    Annealed    650     190    2  80-100-120
            Non-alloy steel   < 0.55 %C  Quenched and   850  250   3            0.30 0.36 0.45  0.48  0.51  0.54 0.57
            and cast steel,             tempered                                0.39  0.45  0.51  0.57  0.60  0.63  0.66
            free cutting steel          Annealed    750     220    4   70-85-100  0.45 0.51 0.57 0.63 0.66 0.69 0.72
                           ≥ 0.55 %C  Quenched and   1000   300    5   50-65-80
          P                             tempered
                                        Annealed    600     200    6   70-90-110
            Low alloy and cast steel (less   Quenched and   930  275  7  70-85-100  0.33 0.36 0.39  0.42  0.45  0.48 0.51
                                                                                0.39
                                                                                     0.42
                                                                                                       0.57
                                                                                                  0.54
                                                                                                            0.60
                                                                                         0.48
                                                                                              0.51
            than 5% of alloying elements)           1000    300    8   50-65-80
                                        tempered                                0.42 0.48 0.54 0.60 0.63 0.66 0.69
                                                    1200    350    9   40-50-60
                                        Annealed    680     200    10  50-70-90  0.27 0.30 0.33  0.36  0.39  0.42 0.45
            High alloyed steel, cast
            steel and tool steel      Quenched and   1100   325    11  40-60-80  0.33  0.36  0.39  0.42  0.45  0.48  0.51
                                        tempered                                0.36 0.39 0.42 0.45 0.48 0.51 0.54
                                     Ferritic / pearlitic   180    15  90-125-140
            Gray cast iron (GG)         Pearlitic /
                                       martensitic          260    16  80-110-120  0.40 0.45 0.54  0.60  0.66  0.72 0.78
          K  Nodular cast iron (GGG)     Ferritic           160    17  90-135-160  0.60  0.66  0.72  0.78  0.84  0.90  0.96
                                        Pearlitic           250    18  80-110-120  0.78 0.84 0.90 0.96 1.02 1.08 1.14
                                         Ferritic           130    19  90-125-140
            Malleable cast iron
                                        Pearlitic           230    20  80-110-120
           Recommended cutting data